tout Kategori
Superalloy

Superalloy


(Superalloy) alyaj wo-tanperati yo divize an twa kalite materyèl: 760 °C materyèl wo-tanperati, 1200 °C materyèl segondè-tanperati ak 1500 °C materyèl segondè-tanperati, ak yon fòs rupture nan 800MPa. Nan lòt mo, li refere a materyèl metal wo-tanperati ki travay pou yon tan long anba 760--1500 ° C ak sèten kondisyon estrès.

760 ℃ segondè tanperati materyèl deformation superalloy

760 ℃ 800MPa klas segondè tanperati materyèl Distribisyon superalloy

760 ℃ 800MPa klas segondè tanperati materyèl poud metaliji superalloy

apèsi sou lekòl la

Superalloy klas:

ASTMGBUNSDINJISplis
GH3030Nimonic75N060752.4951
GH3039
GH3044
GH3128N062192.4855NiCr19Mo9Si
GH4180Nimonic80AN070802.4952

Fòm:

Plak/FèyRod/BarDezabiye / FoilFilForgingsTiyo/TibCustomize

kategori: 

Superalliaj ki baze sou fè 

Superalliaj ki baze sou nikèl 

Superalliaj ki baze sou Cobalt

GH3030(GH30)GH3039(GH39)GH3044(GH44)GH3128(GH128)GH3536(GH536)
GH3625(GH625)GH4033(GH33)GH4037(GH37)GH4049(GH49)GH4133(GH4133B)
GH4169(GH169)GH4220(GH220)GH4698(GH698)GH80AGH90
GH93GH105GH141GH145GH163
GH170GH500GH600GH652GH706
GH710GH738GH742GH901
GH1015(GH15)GH1016(GH16)GH1035(GH35)GH1035A (GH35A)GH1131(GH131)
GH1140(GH140)GH2036(GH36)GH2132(GH132)GH2150(GH150)GH2302(GH302)
GH2696(GH696)GH761GH903GH907
Inquiry